Measurement |
Condition |
Value |
Viscosity |
@ 28 °C (82.4 °F) |
350-410 cps |
Color |
White |
|
Density |
@ 25 °C (77 °F) |
1.145 g/cm³ |
Ec(critical exposure) |
Dp(slop of cure-depth vs.ln(E) curve) |
10.1-10.9 mJ/cm2 |
0.14-0.16 |
ASTM Method |
Property Description |
Value |
ASTM D 638 |
Tensile Modulus |
2835-2896 MPa |
ASTM D 638 |
Tensile Strength at Break |
56-61 MPa |
ASTM D 638 |
Elongation at Break |
4-8% |
ASTM D 648 @66PSI |
Heat Deflection Tempertature |
70-75℃ |
ASTM D 790 |
Flexural Strength |
76-83Mpa |
ASTM D 790 |
Flexural Modulus |
2715-2775Mpa |
ASTM D 256 |
Izod Impact (Notched) |
20-30 J/m |
ASTM D 2240 |
Hardness Shore D |
82-86 |